Description Basic covered NiCrMo alloyed electrode. Low H2-content ≤5 ml/100 g (HD) in the weld metal; very low moisture pickup during long term storage. For high strength fine grained structural steels, for cast steel qualities; weld metal insensitive to cold cracking. Redry = for 2 h at 300 – 350 °C . |
Description
Typical Composition of all-weld Metal
Mechanical Test of weld Metal
Operating Data
Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
Welding Positions
- All, except vertical down
Polarity
- DC (+)