Description This electrode is having core wire with 25 Cr 20 Ni for conducting welding of 1.4845/ASTM310S and similar types of high temperature stainless steels it is strongly recommended to decrease the heat input and the interpass temperature to avoid the risk of hot cracking when welding full austenitic steels and nickel base alloys. |
Description
Typical Composition of all-weld Metal
Mechanical Test of weld Metal
Operating Data
Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
Welding Positions
- All, except vertical down