Description The bare wire is low carbon alloyed austenite with rutile flux coating, high impedance of crack propagation with hard-to- weld materials, austenite- ferrite joints and weld cladding is achieved through the increased ferrite content in the weld metal, good welding properties and very good AC weldability. |
Description
Typical Composition of all-weld Metal
Mechanical Test of weld Metal
Operating Data
Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
Welding Positions
- All, except vertical down
Polarity
- DC (+)